17-4 H1025 Stainless Steel
Stainless steel 17-4 H1025 is stainless steel grade 17-4, also known as 630 alloy that has been heat treated at a temperature between 1015° F and 1035° F for 3.75 hours to 4.25 hours.
![]() |
||